How big a block? If it is too big, it may not be able to support its
own weight and will sag.
Gelatin is readily available and safe. I would look for a bulk supplier
rather than going with the small packages of Knox brand available at
the grocery stores.
John Spevacek
Aspen Research, - www.aspenresearch.com
"Turning Questions into Answers"
Opinions expressed herein are my own and may not represent those of my
employer.
- Next message: Lex Moen: "software peak fitting"
- Previous message: aupward_at_hotmail.com: "Question: water-soluble thickeners"
- In reply to: aupward_at_hotmail.com: "Question: water-soluble thickeners"
- Next in thread: Uncle Al: "Re: Question: water-soluble thickeners"
- Messages sorted by: [ date ] [ thread ]
Relevant Pages
|
|