Hello all, I'm working on electrophoretic deposition of TiO2 from
anhydrous solutions on stainless steel. I have some problems with
adhesion. According to lots of sci. papers in odder to obtain better
TiO2 adhesion on substrate it's recommended to perform thermal
annealing at 450oC temperature. But adhesion is still week, you can
easily scrap it down with fingers. Maybe any body have more ideas about
that?
.