Re: How to reduce radiation in Zircon.
- From: Uncle Al <UncleAl0@xxxxxxxxxxxxx>
- Date: Wed, 25 Apr 2007 07:07:07 -0700
hon123456 wrote:
Dear all,
As I know, some Zircon contains radiation level that is
exceed safety level. I want to find information how to reduce the
radiation level of Zircon. Please suggest any website or resource
that is talking about how to reduce the radiation level of Zircon.
1) Synthesize zircon from precursors not contaminated with
actinides.
2) Mine zircon from sources not contaminated with actinides.
Actinide contamination is interstial in zircon. You cannot get it out
without destroying the zircon. Cooking it with neutrons isn't going
to improve anything.
--
Uncle Al
http://www.mazepath.com/uncleal/
(Toxic URL! Unsafe for children and most mammals)
http://www.mazepath.com/uncleal/lajos.htm#a2
.
- References:
- How to reduce radiation in Zircon.
- From: hon123456
- How to reduce radiation in Zircon.
- Prev by Date: How to reduce radiation in Zircon.
- Next by Date: Re: Acid rain
- Previous by thread: How to reduce radiation in Zircon.
- Next by thread: Re: How to reduce radiation in Zircon.
- Index(es):
Relevant Pages
|