Re: What sucks about flux



On Sun, 07 Aug 2005 11:08:00 -0700, the renowned Chris Carlen
<crobc@xxxxxxxxxxxxxxxxxxxxxxxx> wrote:

> So I invested in 4 rolls of Kester 44 in
>0.015", 0.025", and 0.031" Sn63Pb37 (eutectic is wonderful for PCB
>assembly since it flows and hardens almost instantly), and 0.050"
>Sn60Pb40 a while back for home use.

Does anyone have a particular preference on alloy for hand-soldering
fairly fine-pitch (0.5mm) parts?


Best regards,
Spehro Pefhany
--
"it's the network..." "The Journey is the reward"
speff@xxxxxxxxxxxx Info for manufacturers: http://www.trexon.com
Embedded software/hardware/analog Info for designers: http://www.speff.com
.



Relevant Pages

  • Re: What sucks about flux
    ... >>> So I invested in 4 rolls of Kester 44 in ... > I tried PbSn paste when I first learned to solder SMD, ... >Then I switched to 0.015" Kester Sn63Pb37 with liquid RA flux pen. ... Spehro Pefhany ...
    (sci.electronics.design)
  • Re: Keny Banks Muni Photo
    ... I can't believe how he just flows into and out of everything as if he's ... just out riding on the side walk! ... Just rolls right into a ... MuniSano's Profile: http://www.unicyclist.com/profile/13350 ...
    (rec.sport.unicycling)