steve mew wrote:
>
> Anyone know what the composition is of aluminum tin cans, specifically soda
> cans (coke, pepsi etc) ?
> I was hoping to collect a bunch of them and melt them down in a kiln
>
> Has anybody tried to make homemade Aluminium alloy's ?
>
> Any ideas , advice ?
"Scientific American" maybe a decade ago had an article on
rolling then deep drawing aluminum can alloy. If you melt the
cans you will have a lot of dross from the varnish inside and
out. You also have to worry about air oxidation of the molten
metal.
-- Uncle Al http://www.mazepath.com/uncleal/ (Toxic URL! Unsafe for children and most mammals) http://www.mazepath.com/uncleal/qz.pdf
- Next message: steve mew: "Re: Homemade alloys"
- Previous message: steve mew: "Homemade alloys"
- In reply to: steve mew: "Homemade alloys"
- Next in thread: steve mew: "Re: Homemade alloys"
- Reply: steve mew: "Re: Homemade alloys"
- Messages sorted by: [ date ] [ thread ]