Re: Kurtsite
From: Mark (dad4lou_at_yahoo.com)
Date: 10/19/04
- Previous message: ph11be: "molecular contamination transport"
- In reply to: Andy Dingley: "Re: Kurtsite"
- Next in thread: Pittsburgh Pete: "Re: Kurtsite"
- Reply: Pittsburgh Pete: "Re: Kurtsite"
- Messages sorted by: [ date ] [ thread ]
Date: 18 Oct 2004 21:06:43 -0700
Andy Dingley <dingbat@codesmiths.com> wrote in message news:<umjsm05ljjkf4jg912dgtv00iig27n9tus@4ax.com>...
> On 13 Oct 2004 11:31:55 -0700, thefarmdog@hotmail.com (Brent) wrote:
>
> >Does anyone know anything about the metal Kurtsite (i think thats how
> >its spelled). Aparently its an alloy of lead, aluminum and, zinc.
> >Its is very wear resistant, and yet still quite slippery.
>
> Never heard of it by that name.
>
> In the twenties there were a bunch of zinc-based bearing alloys. They
> seemed to work well, but like the early die-casting alloys they
> suffered from impurites between the grains (lead being one culprit)
> and disintegrated after a few years. As a result, they fell from
> favour.
It's spelled Kirksite and is common material for making molds.
Google: Results 1 - 10 of about 666 for kirksite. (0.07 seconds)
Mark
- Previous message: ph11be: "molecular contamination transport"
- In reply to: Andy Dingley: "Re: Kurtsite"
- Next in thread: Pittsburgh Pete: "Re: Kurtsite"
- Reply: Pittsburgh Pete: "Re: Kurtsite"
- Messages sorted by: [ date ] [ thread ]
Relevant Pages
|
|