Hi, Tom.
Thanks for response.

Substrate is commercial cordierite honeycomb with 400 cpsi.
I tried with 50% solid percent gamma alumina slurry(pH=3.5), after
dipping substrate on slurry for 1 minute, finally air blowing..
Actually am thinking this solid % of 50% is too high..
I don't understanding last question of solid alumina, I'm using gamma
alumina as solid powder and ball milling was applied to adjust to
particle size of 2~10 nm size.