Re: Looking for "kish graphite"
From: cwsachs.dejazzd.com (cwsachs_at_dejazzd.com)
Date: 11/10/04
- Previous message: sanman: "Re: Graphite/Carbon Experts : Graphene"
- In reply to: Alain Couture: "Looking for "kish graphite""
- Next in thread: David Kercsmar: "Re: Looking for "kish graphite""
- Messages sorted by: [ date ] [ thread ]
Date: Wed, 10 Nov 2004 10:34:09 -0500 To: Alain Couture <acouture@cegep-chicoutimi.qc.ca>
You may wish sto check out the following . . .
http://www.2spi.com/catalog/new/hopgsub.shtml