Re: Attaching phosphor to zinc

roy.visser_at_gmail.com
Date: 12/16/04


Date: 16 Dec 2004 10:07:45 -0800

Of course... It is a very logical answer on my question. But that is
only because I have negelected to tell that the created zinc/phosphor
particles have to be be able to resist a temperature of about 350
degrees Celcius. So most glues will not be a solution for my problem.
Moreover any treatment that will change the thermodynamic
characteristics of the zinc will not be favourable in this case.