Re: Sourcing an Acrylic / Plexiglas / Perspex / PMMA adhesive
From: Uncle Al (UncleAl0_at_hate.spam.net)
Date: 01/18/05
- Next message: MK: "Re: re:Tin Whiskers: The Next Y2K Problem"
- Previous message: pritam79_at_rediffmail.com: "Sizing in Carbon Fiber"
- In reply to: jtnospam_at_yahoo.com: "Re: Sourcing an Acrylic / Plexiglas / Perspex / PMMA adhesive"
- Messages sorted by: [ date ] [ thread ]
Date: Tue, 18 Jan 2005 13:05:24 -0800
jtnospam@yahoo.com wrote:
>
> > >
> > > Bostik Tensol #3 - From the specification it seemed this would
> fulfil
> > > the requirements perfectly, however in use it gives of the most
> noxious
> > > vapours.
> >
> > Bubbling is often controllable by degassing. Solvent-containing
> > adhesives in spanning applications will give you shrinkage, bubbling,
> > and usually crazing. You need 100% reactive, filled with dissolved
> > polymer to limit shrinkage and boost viscosity.
> >
> > 1) Degassing. Stirred kettle under reduced pressure, preferably
> > with a viewport. Reduce pressure and you will foam out dissolved
> > air. The trick is to pulse the vacuum to control foaming and
> mimimize
> > loss of volatiles (the reactive monomer). Stir and reduce pressure.
> > When it foams, seal. If the foam breaks under stirring, pull vacuum
> > again until it foams. Seal, break foam, pull vacuum, seal... repeat
> a
> > few times.
> >
> > Many viscous liquids won't break foam with stirring. You can chance
> > adding a breaker like Surfynol - *after* qualifying the bond in bench
> > testing. Unless your engineers are really most sincerely absolutely
> > positive the bond won't be compromised, silicone antifoams are risky.
>
> > A good way to break tough foam is to stop stirring and crack to air.
> > Slam it. Then pump down and stir (in that order - don't beat in more
> > air) and do it again. When the dissolved gas gets lean the foam
> won't
> > support itself. 100 ml is easy. A gallon is no big deal. When you
> > get big it can get slow and nasty.
> >
> > If it is a two-part system, degas separately, mix under reduced
> > pressure, dispense. Atmospheric pressure is 760 torr. Water
> > aspirator will pull 20 torr or less (cold water!). That is good
> > enough if you can move enough gas volume. A mechanical pump will do
> > the trick, of course, but you must trap the acrylic vapors or you
> will
> > seize the pump. Gas conductance varies as the *fourth* power of
> > tubing radius. Evey tubing elbow and valve is a punch to the gut.
> > Acrylic monomer is a fantastic plastic solvent. If you use plastic
> > gas plumbing over long times, be able to inspect a section internally
> > for degradation and deposition.
> >
> > 2) Standard amine cure epoxy turns yellow in light and with age.
> > There are hydrogenated epoxies used in museum restoration that resist
> > yellowing. Epoxies can craze acrylic. Reactive acrylics are
> probably
> > better here. Volatile acrylic monomers are blood toxins. If your
> > folks get blued lips and/or fingernails, it's time to go home for the
> > day - and don't do it again. Don't open yourself to O$HA terrorism.
> > You may need positive ventilation masks in a production environment.
> > It's generally cheaper to individually over-protect the workers than
> > to rebuild the facility to minimum specs. Gloves, of couse -
> > impermeable to acrylic monomer.
> >
> > 3) If outside safety certification comes your way, meet them at
> the
> > gate with your legal counsel and a videocam. Record every minute of
> > the visit with credible witnesses present. Jackbooted State
> > compassion is blunted by admissable evidence that survives
> > cross-examination. A videotape cannot be cross-examined. You need
> > trusted witnesses, too. "We are from the government. We are here to
> > help ourselves to you."
>
> Good tome on degassing, Uncle Al, all I would add is to preheat the two
> components before separate degassing a little, it lowers viscosity and
> helps the amine release dissolved CO2. You were right and I overlooked
> the yellowing and shrinkage issues, thanks for the correction.
> Your experience with the safety Nazis is consistent with mine, but
> with the Feds lately I have seen they have less of a "gotcha" approach
> and more of a cooperative, lets fix the problems approach. Also, in the
> worst state, California, Gov. Terminator has called off the dogs, so to
> speak, trying to save what little industry they have left, but this
> last part is just what I've heard. What have others seen?-Jitney
The Left and the Right alternate excesses. Overall the country is a
miracle as long as it can both slosh and equilibrate. Alas, life is
about point values not averages. Our Gubernator is a gem, but he
can't be everywhere. I've never seen a soldier criticized for killing
enemy. Only the survivors can getcha. No survivors - combatants or
hostile witnesses. If you do not generate waste you need not dispose
of it afterward.
Choice starts at the lowest levels. Product is manufacture as well as
manufactured. Design for overall success starting at the start.
There will be more than enough surprises to keep you entertained as
the project matures to market - and warranty claims thereafter. "8^>)
-- Uncle Al http://www.mazepath.com/uncleal/ (Toxic URL! Unsafe for children and most mammals) http://www.mazepath.com/uncleal/qz.pdf
- Next message: MK: "Re: re:Tin Whiskers: The Next Y2K Problem"
- Previous message: pritam79_at_rediffmail.com: "Sizing in Carbon Fiber"
- In reply to: jtnospam_at_yahoo.com: "Re: Sourcing an Acrylic / Plexiglas / Perspex / PMMA adhesive"
- Messages sorted by: [ date ] [ thread ]