Re: Young's Modulus / Steel / Abnormal values
From: jbuch (jbuch_at_CUTHERErevealed.net)
Date: 01/22/05
- Next message: Ken: "Re: Can aluminum be hardened?"
- Previous message: dmartin_at_newarts.com: "Re: Young's Modulus / Steel / Abnormal values"
- In reply to: dmartin_at_newarts.com: "Re: Young's Modulus / Steel / Abnormal values"
- Next in thread: Gerben Sinnema: "Re: Young's Modulus / Steel / Abnormal values"
- Reply: Gerben Sinnema: "Re: Young's Modulus / Steel / Abnormal values"
- Reply: tfagan: "Re: Young's Modulus / Steel / Abnormal values"
- Messages sorted by: [ date ] [ thread ]
Date: Fri, 21 Jan 2005 23:25:25 -0600
dmartin@newarts.com wrote:
> jbuch wrote:
>
>>Michel PIETTE wrote:
>>
>>>Good morning,
>>>
>>
>>If you go here and look at the slide near the very end.... titled
>>anisotropy....
>>
>>http://www.me.polyu.edu.hk/subject/me3302(yliu)/notes/chapt1.
>>
>>you will find listed the claim that the elastic modulus for Iron in
>
> the
>
>>face edge 100 directions is about 135 Gpa and the modulus for Iron in
>
>
>>the cell diagonal 111 direction is about 273 Gpa.
>>
>>
>>Very nice presentation.
>>
>
>
> Thanks Jim, it is just what I was looking for unfortunately he link is
> broken.
>
Email the author......
mmyliu@polyu.edu.hk
Ask if he will give you the link to his excellent materials notes.
- Next message: Ken: "Re: Can aluminum be hardened?"
- Previous message: dmartin_at_newarts.com: "Re: Young's Modulus / Steel / Abnormal values"
- In reply to: dmartin_at_newarts.com: "Re: Young's Modulus / Steel / Abnormal values"
- Next in thread: Gerben Sinnema: "Re: Young's Modulus / Steel / Abnormal values"
- Reply: Gerben Sinnema: "Re: Young's Modulus / Steel / Abnormal values"
- Reply: tfagan: "Re: Young's Modulus / Steel / Abnormal values"
- Messages sorted by: [ date ] [ thread ]