Work of fracture



Have to give a spiel on materials and I am looking for some figures (however
vague) on the effect of heat treatment on this particularly - work of
fracture vs yield. The most useful materials for examples being:
4130 steel
2024 aluminium
6061 aluminium
7075 aluminium

Googling doesn't seem to give any useful links

Any ideas?
--

regards

jc

LEGAL - I don't believe what I wrote and neither should you. Sobriety and/or
sanity of the author is not guaranteed

EMAIL - jcamp@xxxxxxxxxxx and news@xxxxxxxxxxxx are not valid email
addresses. news2x at perentie is valid for a while.
.



Relevant Pages

  • Work of fracture
    ... Have to give a spiel on materials and I am looking for some figures (however ... The most useful materials for examples being: ... 2024 aluminium ... EMAIL - jcamp@xxxxxxxxxxx and news@xxxxxxxxxxxx are not valid email ...
    (sci.engr.metallurgy)
  • Re: Begging For Knowledge : Lighter Cast Iron Replacement
    ... > However the complication I see with aluminium is one of thermal expansion. ... The design goals are for mass produced engines. ... selection and use of materials in high performance auto racing design. ...
    (sci.materials)
  • Re: Magnetic sheilding
    ... NS> Take a video tape degausser and hold it close to a sheet of aluminium ... materials. ... Ferromagnetism is the most important property for an ... effective magnetic shield. ...
    (sci.electronics.repair)
  • Re: (fucking obviously) OT: Walking sticks
    ... you see blind people using, only stronger and made out of cool ... materials, like aluminium and carbon fibre, cutting down to maybe 30 cm- ...
    (uk.rec.motorcycles)
  • Re: Large Space Colonies and Large Disasters
    ... it's not so good against thermal weapons such as ... layer of aluminium to conduct the heat away. ... The cost of materials once NEOs ...
    (sci.space.policy)