Advice needed regarding Diffusion Coefficient of Mo and Nb in Inconel 625 [or Ni or Ni-Cr]
- From: nfornauman@xxxxxxxxx
- Date: 28 May 2006 11:08:01 -0700
I have laser treated Inconel 625 wrought alloy. As a result there are
Nb and Mo rich dendrites. I want to remove this microsegregation by
heat treating and thus diffusion process would give a homogenous alloy
again. I need diffusion coefficients of Mo and Nb in Inconel 625 alloy.
Can someone refer me to data regarding pre-exponent term Do and Q
(activation energy) of Nb and Mo in Incoenl 625 base matrix, [or in Ni
or Ni-Cr alloy].
I have tried Smithells metals handbook but could not find it.
Regards,
Nauman
.