Hi, can someone help me identify the best way to disperse carbon
nanotubes in epoxy? The volume is relatively small (about 100g to
2000g per batch).
There was a discussion last year about blending Al2O3 nano particles
using Microfluidizer High Shear Processors. It costs too much. A three
roll mill may be a good idea. What is the rough cost? How to use it?