Re: Dispersion of Carbon Nanotubes in Epoxy



On Jun 12, 10:56 am, zzhe...@xxxxxxxxxxx wrote:
Hi, can someone help me identify the best way to disperse carbon
nanotubes in epoxy? The volume is relatively small (about 100g to
2000g per batch).

There was a discussion last year about blending Al2O3 nano particles
using Microfluidizer High Shear Processors. It costs too much. A threeroll mill may be a good idea. What is the rough cost? How to use it?

Thank you.

There are three manufacturers for small lab scale three roll mills.
All three are good for your applications. Charles Ross and Son's costs
about $9-$10 USD. Exakt costs about the same. Torrey Hills model costs
about $4k. I am using a Torrey Hills model. Check out their website at
www.threerollmill.com. Good luck!

.