Re: Dispersion of Carbon Nanotubes in Epoxy
- From: Mark Thorson <nospam@xxxxxxxxx>
- Date: Tue, 12 Jun 2007 14:01:32 -0700
Caulk wrote:
There are three manufacturers for small lab scale three roll mills.
All three are good for your applications. Charles Ross and Son's costs
about $9-$10 USD. Exakt costs about the same. Torrey Hills model costs
about $4k. I am using a Torrey Hills model. Check out their website at
www.threerollmill.com. Good luck!
Even a small roll mill is dangerous. Read the safety
instructions carefully. Keep your fingers away from
the "nip" (the place you feed material into).
.
- Follow-Ups:
- Re: Dispersion of Carbon Nanotubes in Epoxy
- From: Ink Maker
- Re: Dispersion of Carbon Nanotubes in Epoxy
- References:
- Dispersion of Carbon Nanotubes in Epoxy
- From: zzheng5
- Re: Dispersion of Carbon Nanotubes in Epoxy
- From: Caulk
- Dispersion of Carbon Nanotubes in Epoxy
- Prev by Date: Re: Dispersion of Carbon Nanotubes in Epoxy
- Next by Date: EN ISO 3651: Determination of resistance to intergranular corrosion of stainless steels
- Previous by thread: Re: Dispersion of Carbon Nanotubes in Epoxy
- Next by thread: Re: Dispersion of Carbon Nanotubes in Epoxy
- Index(es):
Relevant Pages
|