Re: Dispersion of Carbon Nanotubes in Epoxy



On Jun 12, 2:01 pm, Mark Thorson <nos...@xxxxxxxxx> wrote:
Caulk wrote:

There arethreemanufacturers for small lab scalethreerollmills.
Allthreeare good for your applications. Charles Ross and Son's costs
about $9-$10 USD. Exakt costs about the same. Torrey Hills model costs
about $4k. I am using a Torrey Hills model. Check out their website at
www.threerollmill.com. Good luck!

Even a smallrollmillis dangerous. Read the safety
instructions carefully. Keep your fingers away from
the "nip" (the place you feed material into).

Interesting comments about Microfluidizer. Not sure if it is the best
method. Given the cost of carbon nanotubes and small volume, a small
scale three roll mill is a good way to go.

.